Overtightening High-Performance Liquid Chromatography (HPLC) guard columns to HPLC columns can cause several issues, leading to suboptimal chromatographic performance and potential damage to the equipment.

We offer three distinct direct-connect guard systems: EXP Holders, ROC Holders, and Trident Holders. It depends on the HPLC phase you are using. For more details, please refer here.

How to Choose the Right LC Guard Column

Guard columns are small, protective columns placed before the main analytical column to protect it from sample debris and HPLC system contaminants. Overtightening the guard column can cause physical damage to the PEEK ferrule. Excessive tightening can cause the PEEK ferrule to partially block the inlet frit of the HPLC column causing elevated backpressure. Overtightening can make it extremely challenging to remove the guard column or the HPLC column during maintenance or when switching columns. This difficulty can result in accidental damage to the column threads or the column itself (unable to remove ferrule).

What are the consequences of overtightening on the PEEK ferrule and guard cartridge? Below are some images illustrating the effects of excessive tightening on the components of the Trident guard holder and cartridge.

Figure 1

PEEK ferrule immovably embedded within an HPLC column

PEEK ferrule stuck in the HPLC column
27476

Figure 2

impression on the guard cartridge resulting from excessive tightening

Guard Cartridge inlet side.

Figure 3

PEEK ferrule damaged due to overtightening

Ferrule that has been overtightened

Figure 4

unused PEEK ferrule (catalog # 27476)

 

Figure 1: displays the PEEK ferrule immovably embedded within an HPLC column (column will need to be discarded).

Figure 2: exhibits the impression on the guard cartridge resulting from excessive tightening. 

Figure 3: showcases a photograph of a PEEK ferrule damaged due to overtightening.

Figure 4: illustrates an unused PEEK ferrule (catalog 27476).

To prevent these problems, it is essential to adhere to our guidelines for attaching the guard column to the HPLC column. Usually, hand-tightening should suffice. A wrench may be necessary to ensure a leak-free connection, but it should only be turned an additional 1/8 to ¼ of a rotation beyond hand-tight. Please see the instruction sheets for the three different holders for more details. 

Furthermore, it is equally crucial to routinely inspect and replace the ferrule to maintain effective sealing without the risk of overtightening. You will notice a new ferrule (figure 4) to start to expand and look like figure 3 when it needs to be replaced. Replace ferrule every few times the guard holder is removed or shows signs of wear. 

Replacement ferrules:


EXP Titan Hybrid Ferrule
Ersatz-PEEK-Ferrules für Roc LC Vorsäulenhalter, 3er Pck.
Trident System-Ersatz-Ferrules, PEEK, 10er Pck.

Further information:

Authors

  • Gary Oden

    Gary has 20 years of hands-on experience with chromatography, including SPE, HPLC, and LC/MS instrumentation. He began his chromatography career in the laboratory as a bonding chemist and has served as a study director for PFAS analysis, specializing in both bioanalytical and environmental fields. His work in developing HPLC and LC/MS-MS applications has further broadened his expertise in chromatography. Since 2018, Gary has been a key member of Restek’s European-based technical support team, where he offers expert assistance to customers in overcoming complex analytical challenges.

    View all posts
  • Todd Shaffer
GNBL4726